Microstructural evolution during hot compression of a Ni-base superalloy - dynamic and post-dynamic recrystallization below the secondary carbide solvus temperature

Författare
(Emil Eriksson.)
Genre
theses
Språk
Engelska
Förlag År Ort Om boken ISBN
Department of Physics, Chalmers University of Technology 2021 Sverige, Göteborg x, 60 sidor. ill.